Hastelloy-N
Cladding & StructuralDensity: 8.86 g/cm³
Nickel-molybdenum alloy developed for molten salt compatibility. Primary structural material for the MSRE and proposed MSR designs.
Composition
| Nuclide / Element | Fraction |
|---|---|
| Nickel | 0.710000 |
| Molybdenum | 0.160000 |
| Chromium | 0.070000 |
| Iron | 0.050000 |
| Silicon | 0.005000 |
| Manganese | 0.005000 |
Code output
MCNP
c Hastelloy-N (INOR-8)
c Density: 8.86 g/cm3 (use -8.86 on cell card)
c Weight fractions (nominal composition)
m14 28000.80c -0.7100 $ Ni (balance)
42000.80c -0.1600 $ Mo
24000.80c -0.0700 $ Cr
26000.80c -0.0500 $ Fe
14000.80c -0.0050 $ Si
25055.80c -0.0050 $ MnNotes
Also known as INOR-8 or Alloy N. Developed at ORNL for molten fluoride salt service. Modified Hastelloy-N with Ti additions improves irradiation resistance.